ERYONE Matte PLA Filament, 1.75mm Filament for 3D Printer, 1KG(2.2LBS)/ Spool,

€32,99

colour: Rainbow Macarons

  • Rainbow Macarons
  • Rainbow Watercolor five colors
  • High speed-Black
  • High speed-White
  • High speed-Navy blue
  • High speed-Olive green
  • High speed-Light gray
  • Ruby red
  • Black forest green
  • Yellow
  • Pink
  • Red
  • White
  • aqua blue
  • Black
  • Gray
  • navy blue
  • Olive green
  • Blue lilac
  • Mint Green
  • SKIN
  • RED WAX
  • ARMY GREEN
  • Pottery Red
€32,99
Out of stock

visaamerican expressmastergoogle paypaypalshopify payapple pay

Matte PLA review by Parliamo di Maker


Matte PLA review by INOV3D

Feature:

The surface of the print has a matte (matte) effect, suitable for artwork printing.

Specifications:

  • Filament Diameter: 1.75mm
  • Tolerance: ±0.03mm
  • Printing temperature: 190°C-220°C
  • Heated bed temperature: 55-70°C
  • Printing speed: 30-100mm/s

Store window:



FAQ

1.Q: Why are my threads getting tangled? How can I solve it?

A: Thread knotting is not caused by disorderly or imperfect winding. When making filament, the filament is wound back and forth (left to right and then right to left). Usually there is no knotting of the thread. A common cause of tangles is that the filament end is not fixed in the holes of the spool. The knotting by overlapping or the changed winding direction leads to a knotting of the filament. Therefore, customers need to attach the thread end to the correct holes of the bobbin.

2.Q: Can PLA be used for tableware printing?

A: Not recommended. Although PLA is a degradable, food-grade raw material, the PLA with toner is not food-grade.

3.Q: The nozzle is clogged by PLA, how can I solve the problem?

A: An inconstant filament diameter, a nozzle temperature that is too low and frequent replacement with other filaments lead to this problem. So clean the nozzle before you start and adjust the temperature to a reasonable level.

4.Q: My prints have problems with web-like threads (stringing). How can I fix the problem?

A: If the temperature is too high, the PLA filament will melt and flow so quickly. Please lower the temperature to a reasonable level. The retract parameters are incorrect, so adjust the retract length and speed.

5.Q: There is too much melted filament around the nozzle. What should I do?

A: This issue can be traced back to too high temperature, too low print speed, and nozzle diameter mismatch in slice software with extrusion performance.

6.Q: The PLA filament was perfect when I opened the package. After printing intermittently several times, my PLA filament accidentally breaks during printing. Why?

A: Normally, PLA filament does not break by itself during the printing process. However, being a degradable material, PLA becomes more brittle and breaks easily after exposure to moisture, so you should pay attention to moisture protection.

7.Q: The surface of my print is not very smooth and the extruded filament has inconstant diameters. Why is that?

A: The printing temperature is too high or too low. The temperature does not match the print speed. You need to adjust the print speed or temperature.

8.Q: Why won't my PLA printed objects stick to the heatbed? How can I solve this?

A: The distance between the nozzle and the bed is too big. Make sure your heatbed is level and clean. Then judge whether the printing temperature and heatbed temperature are too low, and our customers should adjust them to the right range.

Sunday,Monday,Tuesday,Wednesday,Thursday,Friday,Saturday
January,February,March,April,May,June,July,August,September,October,November,December
Not enough items available. Only [max] left.
Add to WishlistBrowse WishlistRemove Wishlist
Shopping cart

Your cart is empty.

Return To Shop

Add Order Note Edit Order Note
Estimate Shipping
Add A Coupon

Estimate Shipping

Add A Coupon

Coupon code will work on checkout page

English

Select your language

EUR

Select your currency

ERYONE Matte PLA Filament, 1.75mm Filament for 3D Printer, 1KG(2.2LBS)/ Spool,

Rainbow Macarons
Rainbow Macarons
€32,99