Features:
- Along with the galaxy powder, it looks super dazzling with the metal powder spray texture.
- Compared to the usual pearl powder and galaxy powder, our special galaxy powder has a fine and smooth texture, a smaller particle size, a uniform distribution, a lower clogging rate.
- Universal compatibility with 99% of popular FDM 3D printers.
- Less laminate abrasion, smoother print surface.
- Eco-friendly, non-toxic, degradable.
Specifications:
- Filament Diameter: 1.75mm
- Tolerance: ±0.03mm
- Printing temperature: 190°C-220°C
- Heated bed temperature: 55-70°C
- Printing speed: 30-60mm/s
showcase:
FAQ
1.Q: Why are my threads getting tangled? How can I solve it?
A: Thread knotting is not caused by disorderly or imperfect winding. When making filament, the filament is wound back and forth (left to right and then right to left). Usually there is no knotting of the thread. A common cause of tangles is that the filament end is not fixed in the holes of the spool. The knotting by overlapping or the changed winding direction leads to a knotting of the filament. Therefore, customers need to attach the thread end to the correct holes of the bobbin.
2.Q: Can PLA be used for tableware printing?
A: Not recommended. Although PLA is a degradable, food-grade raw material, the PLA with toner is not food-grade. If you really want to print on a tableware, transparent PLA is recommended.
3.Q: The nozzle is clogged by PLA, how can I solve the problem?
A: An inconstant filament diameter, a nozzle temperature that is too low and frequent replacement with other filaments lead to this problem. So clean the nozzle before you start and adjust the temperature to a reasonable level.
4.Q: My prints have problems with web-like threads (stringing). How can I fix the problem?
A: If the temperature is too high, the PLA filament will melt and flow so quickly. Please turn down the temperature to a reasonable level.
The feed parameters are not correct, so adjust the feed length and speed.
5.Q: My prints have problems with web-like threads (stringing). How can I fix the problem?
A: The feed parameters are not correct, so adjust the feed length and speed.
6.Q: The PLA filament was perfect when I opened the package. After printing intermittently several times, my PLA filament accidentally breaks during printing. Why?
A: Normally, PLA filament does not break by itself during the printing process. However, being a degradable material, PLA becomes more brittle and breaks easily after exposure to moisture, so you should pay attention to moisture protection.
7.Q: The surface of my print is not very smooth and the extruded filament has inconstant diameters. Why is that?
A: The printing temperature is too high or too low. The temperature does not match the print speed. You need to adjust the print speed or temperature.
8.Q: Why won't my PLA printed objects stick to the heatbed? How can I solve this?
A: The distance between the nozzle and the bed is too big. Make sure your heatbed is level and clean. Then judge whether the printing temperature and heatbed temperature are too low, and our customers should adjust them to the right range.